Fe2O3solwiththeparticlediameterof3-5nmwasflocculatedbytheadditionofSDS,andtheflocculateformedwasredispersedbythefurtheradditionofthatsurfactant.ThusthesurfactantbilayerwasformedonthesurfaceofFe2O3.Theemulsionpolymerizationofstyrene(St)adsolubilizedonthesurfactantadsorbedbilayerwascarriedoutbyinitiatorpotassiumpersulfate(KPS).TheUV-Visandsurfacephotovoltagespectra(SPS)indicatethattheFe2O3particleswereencapsulatedinpolystyrene(PSt)successfully.