Calcified roasting-acid leaching process of vanadium from low-grade vanadium-containing stone coal

在线阅读 下载PDF 导出详情
摘要 Thelow-gradevanadium-containingstonecoalusedinthisexperimentwascollectedfromWuxiCountry,ChongqingCity,China.Theexperimentfocusedonthevanadiumrecoveryfromroastedresiduethroughoptimizingtheprocessconditionsofaneffectiveandenvironmentally-friendlytechnology,namedcalcifiedroasting-sulfuricacidleachingtechnology.Bysingle-factorexperimentsandorthogonalexperiments,theeffectsofroastingtemperature,roastingtime,sulfuricacidconcentrationandleachingtimeontheleachingratioofvanadiumwereanalyzed.Theresultsshowedthattheleachingratioofvanadiumreached85.5%underthepropertechnologicalconditionsofroastingtemperature=950℃,roastingtime=4h,40%concentrationofsulfuricacidandleachingtime=6h.